Flow Lines

Flow lines present as irregular shallow round or angular grooves that appear on the surface of the casting. This defect indicates that the ceramic shell was built around a defective wax pattern. 

 

The causes of this defect are evident in the wax portion of the process. To cure these causes, R&R recommends taking the following actions.